Fig. 2 Image of surface layer cross-section of fusion reactor structural material (Reduced activation ferritic martensitic steel) immersed in liquid tin. (IMAGE)
Caption
(a) When immersed in liquid tin at 500°C for 25 hours. (b) When immersed in liquid tin at 500°C for 250 hours. Taken using a scanning electron microscope.
Credit
Masatoshi Kondo