Fig.3 Image of cross-section of surface layer corrosion structure of oxide sinter immersed in liquid metal tin (IMAGE)
Caption
(a) When a sintered body of iron oxide (Fe2O3) was immersed in liquid tin at 500°C for 262 hours. (b) When a sintered body of chromium oxide (Cr2O3) was immersed in liquid tin at 500°C for 262 hours. Images obtained using a scanning electron microscope.