Honeycomb structure with oxygen-poor pores at the top of magnetite layer on a martensitic steel CLAM exposed to lead-bismuth eutectic at 500 ºC (IMAGE)
Caption
(a) Cross-sectional morphology of steel exposed to LBE containing 10-7 wt% oxygen for 2000 h. (b)-(f) EDS map scanning results of the area indicated by the blue box in (a).