Some of the wear and tear from battle that occurred during the experiment with controlled impacts on the replica bronze spearheads: (A–B) Notch with burr, side & top view (C–D) Notch with burr, side & top view (E–F) Bowing dent with trail, side & to (IMAGE)
Caption
Some of the wear and tear from battle that occurred during the experiment with controlled impacts on the replica bronze spearheads: (A–B) Notch with burr, side and top view. (C–D) Notch with burr, side and top view. (E–F) Bowing dent with trail, side and top view. (G–H) Bowing dent with trails, side and top view
Credit
Valerio Gentile, available via cc licence from https://doi.org/10.1016/j.jas.2024.106044
Usage Restrictions
None
License
Original content