Enhanced thermal stability in the studied alloys with the addition of cobalt (IMAGE)
Caption
Enhanced thermal stability in the studied alloys with the addition of cobalt (0, 15, and 30 atomic per cent (at.%)). a–c Typical SEM micrographs of nanoparticles in the three chemically complex alloys aged at 1000 °C for 240 h, and their average diameter. d–f The evolution of the average size of nanoparticles in the three chemically complex alloys aged at 800, 900, and 1000 °C for different durations (24 h, 72 h, 168 h and 240 h).
Credit
Xiao, B. et al, (source: https://www.nature.com/articles/s41467-022-32620-6)